Material | NdFeB |
Grade | N40M |
Remanence Br(kGs) |
Max:12.8 Min:12.5 |
Plating | Ni-Cu-Ni (Nickel) |
Shape | Disc |
Coercive force(kOe) Min. | 11.6 |
Intrinsic Coercive force (kOe) Min. | 14 |
Max energy product (MGOe) |
Max:41 Min:38 |
Max Temp (℃) | 100 |