Material | NdFeB |
Grade | N33SH |
Remanence Br(kGs) |
Max:11.7 Min:11.3 |
Plating | Ni-Cu-Ni (Copper) |
Shape | Segment |
Coercive force(kOe) Min. | 10.6 |
Intrinsic Coercive force (kOe) Min. | 20 |
Max energy product (MGOe) |
Max:34 Min:31 |
Max Temp (℃) | 150 |